Thermal fatigue cracking of surface engineered hot work tool steels A Persson, S Hogmark, J Bergström Surface and Coatings Technology 191 (2-3), 216-227, 2005 | 254 | 2005 |
Simulation and evaluation of thermal fatigue cracking of hot work tool steels A Persson, S Hogmark, J Bergström International Journal of Fatigue 26 (10), 1095-1107, 2004 | 186 | 2004 |
Thermal fatigue testing of chromium martensitic hot-work tool steel after different austenitizing treatments J Sjöström, J Bergström Journal of materials processing technology 153, 1089-1096, 2004 | 154 | 2004 |
High-temperature properties and microstructural stability of hot-work tool steels A Medvedeva, J Bergström, S Gunnarsson, J Andersson Materials Science and Engineering: A 523 (1-2), 39-46, 2009 | 153 | 2009 |
Microstructural characterization and wear behavior of (Fe, Ni)–TiC MMC prepared by DMLS A Gåård, P Krakhmalev, J Bergström Journal of Alloys and Compounds 421 (1-2), 166-171, 2006 | 143 | 2006 |
Temperature effects on adhesive wear in dry sliding contacts A Gåård, N Hallbäck, P Krakhmalev, J Bergström Wear 268 (7-8), 968-975, 2010 | 98 | 2010 |
Tribological simulation of aluminium hot extrusion T Björk, J Bergström, S Hogmark Wear 224 (2), 216-225, 1999 | 94 | 1999 |
Physical vapour deposition duplex coatings for aluminium extrusion dies T Björk, R Westergård, S Hogmark, J Bergström, P Hedenqvist Wear 225, 1123-1130, 1999 | 86 | 1999 |
Failure modes in field-tested brass die casting dies A Persson, S Hogmark, J Bergström Journal of Materials Processing Technology 148 (1), 108-118, 2004 | 80 | 2004 |
Temperature profiles and conditions for thermal fatigue cracking in brass die casting dies A Persson, S Hogmark, J Bergström Journal of materials processing technology 152 (2), 228-236, 2004 | 67 | 2004 |
Influence of deposition temperature and time during PVD coating of CrN on corrosive wear in liquid aluminium A Persson, J Bergström, C Burman, S Hogmark Surface and Coatings Technology 146, 42-47, 2001 | 66 | 2001 |
Atomistic insights on the wear/friction behavior of nanocrystalline ferrite during nanoscratching as revealed by molecular dynamics AT AlMotasem, J Bergström, A Gåård, P Krakhmalev, LJ Holleboom Tribology letters 65, 1-13, 2017 | 61 | 2017 |
Galling resistance and wear mechanisms–cold work tool materials sliding against carbon steel sheets A Gåård, PV Krakhmalev, J Bergström, N Hallbäck Tribology letters 26, 67-72, 2007 | 61 | 2007 |
Wear mechanisms in deep drawing of carbon steel–correlation to laboratory testing A Gåård, P Krakhmalev, J Bergström Tribotest 14 (1), 1-9, 2008 | 60 | 2008 |
Characterization of an iron-based laser sintered material Y Wang, J Bergström, C Burman Journal of Materials Processing Technology 172 (1), 77-87, 2006 | 59 | 2006 |
Influence of tool steel microstructure on origin of galling initiation and wear mechanisms under dry sliding against a carbon steel sheet A Gåård, P Krakhmalev, J Bergström Wear 267 (1-4), 387-393, 2009 | 58 | 2009 |
Thermal fatigue in hot‐working tools J Sjöström, J Bergström Scandinavian Journal of Metallurgy 34 (4), 221-231, 2005 | 55 | 2005 |
Galling resistance and wear mechanisms for cold-work tool steels in lubricated sliding against high strength stainless steel sheets P Karlsson, A Gåård, P Krakhmalev, J Bergström Wear 286, 92-97, 2012 | 54 | 2012 |
Relaxation of shot peening induced compressive stress during fatigue of notched steelsamples J Bergström, T Ericsson Surface Engineering 2 (2), 115-120, 1986 | 44 | 1986 |
Very high cycle fatigue of cold rolled stainless steels, crack initiation and formation of the fine granular area MW Tofique, J Bergström, K Svensson International Journal of Fatigue 100, 238-250, 2017 | 43 | 2017 |