Testing the chloride penetration resistance of concrete: a literature review
KD Stanish, RD Hooton, MDA Thomas
United States. Federal Highway Administration, 2001
3462001
Performance of cement-based materials in aggressive aqueous environments
M Alexander, A Bertron, N De Belie
Springer 10, 462, 2013
2992013
Durability of ternary blend concrete with silica fume and blast-furnace slag: laboratory and outdoor exposure site studies
R Bleszynski, RD Hooton, MDA Thomas, CA Rogers
ACI Materials Journal-American Concrete Institute 99 (5), 499-508, 2002
2452002
Reactivity tests for supplementary cementitious materials: RILEM TC 267-TRM phase 1
X Li, R Snellings, M Antoni, NM Alderete, M Ben Haha, S Bishnoi, Ö Cizer, ...
Materials and Structures 51, 1-14, 2018
2032018
Effect of limestone filler on the deterioration of mortars and pastes exposed to sulfate solutions at ambient temperature
ST Lee, RD Hooton, HS Jung, DH Park, CS Choi
Cement and concrete research 38 (1), 68-76, 2008
1852008
Canadian use of ground granulated blast-furnace slag as a supplementary cementing material for enhanced performance of concrete
RD Hooton
Canadian Journal of Civil Engineering 27 (4), 754-760, 2000
1802000
RILEM TC-238 SCM recommendation on hydration stoppage by solvent exchange for the study of hydrate assemblages
R Snellings, J Chwast, Ö Cizer, N De Belie, Y Dhandapani, P Durdzinski, ...
Materials and structures 51, 1-4, 2018
1642018
Report of TC 238-SCM: hydration stoppage methods for phase assemblage studies of blended cements—results of a round robin test
R Snellings, J Chwast, Ö Cizer, N De Belie, Y Dhandapani, P Durdzinski, ...
Materials and structures 51, 1-12, 2018
1632018
Properties and durability of concrete produced using CO2 as an accelerating admixture
S Monkman, M MacDonald, RD Hooton, P Sandberg
Cement and Concrete Composites 74, 218-224, 2016
1412016
Design for durability: The key to improving concrete sustainability
RD Hooton, JA Bickley
Construction and Building Materials 67, 422-430, 2014
1322014
The deleterious chemical effects of concentrated deicing solutions on Portland cement concrete
L Sutter, K Peterson, G Julio-Betancourt, D Hooton, TV Dam, K Smith
South Dakota Department of Transportation, Office of Research, 2008
1282008
Re-evaluation of the AASHTO T259 90-day salt ponding test
PF McGrath, RD Hooton
Cement and Concrete Research 29 (8), 1239-1248, 1999
1241999
Alkali-aggregate reaction in concrete: A world review
I Sims, A Poole
CRC Press, 2017
1192017
Reduction in mortar and concrete expansion with reactive aggregates due to alkali leaching
CA Rogers, RD Hooton
Cement, Concrete, and Aggregates 13 (1), 42-49, 1991
1071991
Sulfate resistance of a Canadian slag cement
RD Hooton, JJ Emery
Materials Journal 87 (6), 547-555, 1990
851990
Supplementary cementitious materials for concrete: characterization needs
M Juenger, JL Provis, J Elsen, W Matthes, RD Hooton, J Duchesne, ...
MRS Online Proceedings Library (OPL) 1488, imrc12-1488-7b-026, 2012
822012
Field trials of concretes produced with portland limestone cement
MDA Thomas, D Hooton, K Cail, BA Smith, J De Wal, KG Kazanis
Concrete international 32 (1), 35-41, 2010
802010
Alkali-aggregate reactions in Ontario
C Rogers, PE Grattan-Bellew, RD Hooton, J Ryell, MDA Thomas
Canadian Journal of Civil Engineering 27 (2), 246-260, 2000
712000
Ground granulated blast-furnace slag
W Matthes, A Vollpracht, Y Villagrán, S Kamali-Bernard, D Hooton, ...
Properties of Fresh and Hardened Concrete Containing Supplementary …, 2018
682018
Glass content determination and strength development predictions for vitrified blast furnace slag
RD Hooton, JJ Emery
Special Publication 79, 943-962, 1983
661983