Magnetorheological methods for nanofinishing–a review
TS Bedi, AK Singh
Particulate Science and Technology 34 (4), 412-422, 2016
822016
Modeling and simulation of surface roughness in magnetorheological fluid based honing process
SK Paswan, TS Bedi, AK Singh
Wear 376, 1207-1221, 2017
642017
A new magnetorheological finishing process for ferromagnetic cylindrical honed surfaces
TS Bedi, AK Singh
Materials and Manufacturing Processes 33 (11), 1141-1149, 2018
272018
Development of magnetorheological fluid-based process for finishing of ferromagnetic cylindrical workpiece
TS Bedi, AK Singh
Machining Science and Technology 22 (1), 120-146, 2018
272018
Spot nanofinishing using ball nose magnetorheological solid rotating core tool
A Khurana, AK Singh, TS Bedi
The International Journal of Advanced Manufacturing Technology 92, 1173-1183, 2017
132017
Fine-finishing of stepped cylindrical workpiece using magnetorheological finishing process
AS Rana, TS Bedi, V Grover
Materials Today: Proceedings 41, 886-892, 2021
102021
An initial new approach for magnetorheological finishing of ferromagnetic internal cylindrical surfaces
TS Bedi, AK Singh
The International Journal of Advanced Manufacturing Technology 100, 1017-1030, 2019
92019
Magnetorheological finishing of ferromagnetic blind-hole type surfaces
TS Bedi, AK Singh
Materials and Manufacturing Processes 33 (11), 1169-1176, 2018
92018
Comparative performance of magnetorheological external finishing tools using different magnetic structures
TS Bedi, R Kant
Materials Today: Proceedings 41, 908-914, 2021
72021
Surface finishing requirements on various internal cylindrical components: A review
TS Bedi, AS Rana
Journal of Micromanufacturing 4 (2), 216-228, 2021
42021
A new permanent magnet type magnetorheological finishing tool for external cylindrical surfaces having different outer diameter
AS Rana, TS Bedi, V Grover
Advances in Production and Industrial Engineering: Select Proceedings of …, 2020
42020
Strength analysis of rotary friction welded joints of dissimilar steel grades
JS Chatha, A Handa, TS Bedi
Materials Today: Proceedings 38, 242-247, 2021
32021
Advanced Finishing Processes for Biomedical Applications
TS Bedi, R Kant, H Gurung
Advanced Micro-and Nano-manufacturing Technologies: Applications in …, 2022
22022
Parametric study of a newly developed magnetorheological honing process
TS Bedi, AK Singh
Advances in Unconventional Machining and Composites: Proceedings of AIMTDR …, 2019
22019
Corrosion Studies on HVOF Sprayed Ni-20Cr and Ni-50Cr Coatings on ASTM A213 TP347H Boiler Steel at 700 degree Celsius
TS Bedi, SS Aulakh, G Kaushal
Asian Review of Mechanical Engineering 2 (2), 56-60, 2013
22013
Parametric optimization of curved-rectangular shaped magnetorheological finishing tool for external cylindrical surfaces
AS Rana, I Rafiq, TS Bedi
E3S Web of Conferences 430, 01263, 2023
12023
Hot corrosion studies on HVOF sprayed Ni-20Cr coated ASTM A213 TP347H boiler steel at 700 C
TS Bedi, JS Gill, G Kushal
International Conference on Advancements and Futuristic Trends in Mechanical …, 2014
12014
Rotary Friction Welding of Dissimilar Materials
JS Chatha, TS Bedi, A Handa
International Journal of Recent Technology and Engineering (IJRTE) ISSN …, 0
1
Improved approach to magnetorheological finishing of blind-hole cavities
TS Bedi, SK Pawan, R Kant, AS Rana
Materials and Manufacturing Processes, 1-8, 2024
2024
Parametric approach of magnetorheological external finishing tool for its better functionality
AS Rana, TS Bedi, H Gurung
Modern Materials and Manufacturing Techniques, 96-119, 2024